Austenitic stainless
1.4539 Alloy 904L X1CrNiMoCu25-20-5
High-alloy super-austenitic with elevated nickel, molybdenum and copper for resistance to sulphuric and phosphoric acid and seawater; low carbon secures weld corrosion resistance.
Download data sheet (PDF)Availability
Per our product catalogueOur product catalogue lists no sizes in 1.4539. Send us an enquiry for this grade directly.
Chemical composition
mass %| Element | Content |
|---|---|
| CCarbon | ≤0.02 |
| SiSilicon | ≤0.7 |
| MnManganese | ≤2 |
| PPhosphorus | ≤0.03 |
| SSulphur | ≤0.01 |
| NNitrogen | ≤0.15 |
| CrChromium | 19–21 |
| CuCopper | 1.2–2 |
| MoMolybdenum | 4–5 |
| NiNickel | 24–26 |
Mechanical properties
room temperature- Rp0.2 min (N/mm²)
- 230
- Rp1.0 min (N/mm²)
- 250
- Rm (N/mm²)
- 520–720
- Elongation A% (longitudinal)
- 35
- Elongation A% (transverse)
- 30
- Impact energy KV J (longitudinal)
- 120
- Impact energy KV J (transverse)
- 90
Seamless tube.
Standard equivalences
- DIN/EN
- X1CrNiMoCu25-20-5
- AISI
- 904L
- UNS
- N08904
- SS
- 2562
- AFNOR
- Z1 NCDU 25.20
- BS
- 904 S13
- PN
- 0H22N24M4TCa
Typical applications
- Chemical plant and oil refineries
- Petrochemical plant
- Paper-industry bleach tanks
- Flue-gas desulphurisation
- Seawater, sulphuric- and phosphoric-acid service
Frequently asked questions
What is 1.4539 (Alloy 904L)?
1.4539 (X1CrNiMoCu25-20-5) — Austenitic stainless. High-alloy super-austenitic with elevated nickel, molybdenum and copper for resistance to sulphuric and phosphoric acid and seawater; low carbon secures weld corrosion resistance.
Which grades are equivalent to 1.4539?
1.4539 corresponds to EN X1CrNiMoCu25-20-5; equivalent designations: AISI 904L, UNS N08904, SS 2562, AFNOR Z1 NCDU 25.20, BS 904 S13, PN 0H22N24M4TCa.
Related grades
Indicative values — verify against the applicable standard before specifying.