Ferritic heat-resistant
1.4713 X10CrAl7
Aluminium-alloyed ferritic heat-resistant steel, particularly resistant to sulphur-bearing gases at elevated temperature under reducing conditions.
Download data sheet (PDF)Availability
Per our product catalogueOur product catalogue lists no sizes in 1.4713. Send us an enquiry for this grade directly.
Chemical composition
mass %| Element | Content |
|---|---|
| CCarbon | ≤0.12 |
| SiSilicon | 0.5–1 |
| MnManganese | ≤1 |
| PPhosphorus | ≤0.04 |
| SSulphur | ≤0.03 |
| AlAluminium | 0.5–1 |
| CrChromium | 6–8 |
Mechanical properties
room temperature- Scaling temperature (°C)
- 800
Standard equivalences
- DIN/EN
- X10CrAl7
- AFNOR
- Z8 CA 7
Typical applications
- Furnaces and gas turbines
- Exhaust valves and thermowell tubes
- Power-plant and reactor construction
- Heat exchangers, muffle tubes, recuperators
Frequently asked questions
What is 1.4713 (—)?
1.4713 (X10CrAl7) — Ferritic heat-resistant. Aluminium-alloyed ferritic heat-resistant steel, particularly resistant to sulphur-bearing gases at elevated temperature under reducing conditions.
Which grades are equivalent to 1.4713?
1.4713 corresponds to EN X10CrAl7; equivalent designations: AFNOR Z8 CA 7.
Related grades
Indicative values — verify against the applicable standard before specifying.