Austenitic heat-resistant
1.4841 TP 314 X15CrNiSi25-21
Heat-resistant austenitic Cr-Ni steel with good scaling resistance and high hot strength, for duty needing both oxidation resistance and mechanical load capacity.
Download data sheet (PDF)Availability
Per our product catalogueOur product catalogue lists no sizes in 1.4841. Send us an enquiry for this grade directly.
Chemical composition
mass %| Element | Content |
|---|---|
| CCarbon | ≤0.2 |
| SiSilicon | 1.5–2.5 |
| MnManganese | ≤2 |
| PPhosphorus | ≤0.045 |
| SSulphur | ≤0.03 |
| CrChromium | 24–26 |
| NiNickel | 19–22 |
Mechanical properties
room temperature- Scaling temperature (°C)
- 1150
Standard equivalences
- DIN/EN
- X15CrNiSi25-21
- AISI
- 314
- UNS
- S31400
- AFNOR
- Z12 CNS 20.20
- BS
- 314 S25
- PN
- H25N20S2
Typical applications
- Industrial furnace and apparatus construction
- Thermowell tubes
- Steelworks and smelters
- Air preheaters, recuperators, furnace tubes
Frequently asked questions
What is 1.4841 (TP 314)?
1.4841 (X15CrNiSi25-21) — Austenitic heat-resistant. Heat-resistant austenitic Cr-Ni steel with good scaling resistance and high hot strength, for duty needing both oxidation resistance and mechanical load capacity.
Which grades are equivalent to 1.4841?
1.4841 corresponds to EN X15CrNiSi25-21; equivalent designations: AISI 314, UNS S31400, AFNOR Z12 CNS 20.20, BS 314 S25, PN H25N20S2.
Related grades
Indicative values — verify against the applicable standard before specifying.