Ferritic heat-resistant
1.4761
X8CrTi25 mod.
High-chromium titanium-stabilised, nickel-free ferritic heat-resistant steel with good resistance to sulphurous atmospheres. Continuous use in the 400–700 °C range is not recommended.
Chemical composition
mass %| Element | Content |
|---|---|
| CCarbon | ≤0.15 |
| SiSilicon | ≤1 |
| MnManganese | ≤0.8 |
| CrChromium | 24–27 |
| TiTitanium | 5×C – 0.9 |
Mechanical properties
room temperature- Scaling temperature (°C)
- 1100
Standard equivalences
- DIN/EN
- X8CrTi25 mod.
- PN
- H25T
- Source datasheet header reads '1.4746 mod.'; the cross-reference table and index list it as 1.4761.
Typical applications
- Furnaces, exhaust systems, exhaust valves
- Heat exchangers and heat-resistant tube
- Cement, gypsum, glass works, smelters
- Food industry
Frequently asked questions
What is 1.4761 (—)?
1.4761 (X8CrTi25 mod.) — Ferritic heat-resistant. High-chromium titanium-stabilised, nickel-free ferritic heat-resistant steel with good resistance to sulphurous atmospheres. Continuous use in the 400–700 °C range is not recommended.
Which grades are equivalent to 1.4761?
1.4761 corresponds to EN X8CrTi25 mod.; equivalent designations: PN H25T.
Related grades
Indicative values — verify against the applicable standard before specifying.
Request this grade